Lithium ion battery
Example of laser drilling on LIB positive electrode by sheet laser machining machine
Introduces examples of drilling holes in the LIB positive electrode using a sheet laser machine.
The LIB positive electrode (t = 130 μm) was machined with a hole diameter of 12 μm, a pitch of 110 μm (parallel), and an aperture ratio of 0.9%.
Processing with a roll-to-roll laser processing machine is also possible. WIRED Co., Ltd.
Example of laser drilling in LIB negative electrode by sheet laser machining machine
Introduces examples of drilling holes in the LIB negative electrode using a sheet laser machine.
The LIB negative electrode (t = 130 μm) was machined with a hole diameter of 16 μm, a pitch of 110 μm (parallel), and an aperture ratio of 1.5%.